Vacuum Casting processing services for prototype Custom

What is vacuum casting prototype?

Silicone replication is an economical and efficient alternative solution for small-scale plastic parts production, which can accurately replicate the final molded parts or finished products. Usually, we use silicone rubber to make molds and combine them with CNC or SLA parts as master molds.

These molds are capable of replicating all the structural and surface features of a product, and the overmolding can be used to replicate another product. A set of silicone molds can usually replicate 10-15 sets of products.

Silicone replication production process

Model making

Based on your 3D drawings, we will use CNC machining and 3D printing (SLS/SLA) technology to produce the main parts. For parts with complex shapes and structures, we will also consider using SLA technology to make molds.

Silicone mold production

We will inject silicone around the mold and then use a vacuum process to remove all air. Next, place the mold in a 40 ℃ oven for curing. The curing time will depend on the low volume of the mold and generally takes 8-16 hours.

Vacuum film coating

We pour the resin into the mold in the vacuum chamber through computer control, and then put it back into the oven for curing. In general, the curing time for small components is 1-3 hours, while large components require 3-6 hours. After curing, we will remove the cast parts from the silicone mold and prepare for the next cycle.

Silicone Vacuum Casting processing
Silicone Vacuum Casting processing
Silicone Vacuum Casting processing
Silicone Vacuum Casting processing

Material selection for vacuum casting

Explore premium silicone vacuum casting materials for polyurethane, ABS-like, and transparent resins. Ideal for rapid prototyping & low-volume production. Fast curing & high detail.

vacuum casting Prototype and Parts Display

The products displayed below have been approved by the customer, and we strictly abide by the confidentiality agreement to protect the customer’s confidentiality and creativity.

Silicone Mold Duplication Technology Guide

Standard accuracy: The standard tolerance is ±0.15 mm/100 mm, with a maximum accuracy of ±0.05 mm.

Maximum part size: The vacuum equipment can accommodate mold specifications of 1.8 m × 1.2 m × 1.0 m.

Minimum wall thickness: The minimum wall thickness is 0.5 mm, and the recommended thickness is between 1.5 mm and 2.5 mm.

Standard delivery time: Up to 50 pieces can be produced within 7 to 10 days, depending on part specifications and quantity.

Service life of silicone molds: Each mold can produce up to 20 castings, but if the parts have high requirements, such as clear or complex structures, then one mold can only produce 12 or even 10 castings.

Surface finish and other functions: Coloring, texturing, painting, coating, transparent polishing, embedding, and over-molding.

Advantages of silicone vacuum casting

Advantages of silicone vacuum casting

  • An economical and efficient method for producing small to medium batches of plastic parts.
  • Multiple materials, including polyurethane, epoxy, and soft silicone.
  • The preferred choice for functional prototypes and finished products.
  • Low mold costs.
  • Fast turnaround times.
silicone vacuum casting application

silicone vacuum casting application

Silicone molding is suitable for the production of small to medium batches of high-quality, low-cost, and precise plastic parts.

  • Automotive industry: Dashboard components, door handles, and interior parts.
  • Industrial: Aircraft bodies, structural/functional parts
  • Medical industry: Computer electronics shells, chassis and parts, brackets, cabinets

Why choose our silicone vacuum casting services?

We offer a variety of manufacturing solutions to meet different needs, from sample customization to small-batch production.

Our quality system has obtained ISO 9001:2015 international certification.

Each silicone mold can produce 15 to 18 castings, and the production time depends on the scale and standards of the project, usually completed within 7 to 10 days.

We have strong production capabilities, so we can flexibly arrange production cycles to meet your various product production needs.