Nitralloy 135 Stainless Steel: Properties, Uses & Manufacturing Guide
Nitralloy 135 stainless steel is a nitrogen-alloyed, martensitic stainless steel designed for applications requiring a combination of high strength, good corrosion resistance, and reliable performance at elevated temperatures. The addition of nitrogen (0.10-0.20%) is the key differentiator, boosting its tensile strength and fatigue resistance without compromising its corrosion resistance or weldability. This makes it a […]